Hi guys!
I'm here again.

I'm organizing PWHT requirement using excel.
I have to write only one thickness on a excel table.
My team leader said the table makes people so confused because of two thickness(control thickness, nominal thickness) on one table.
Example of the table is like this.
-Example(from B31.1)-
P No. Thickness PWHT Temperature
=========================================================================
P-15E 13Tn<Pipe<=50Tc 705~775℃
(P-91,92)

cf)Tn means nominal thickness and Tc means control thickness

So I decided convert control thickness to nominal thickness.

The reason of converting is PWHT temperature and PWHT exemption requirement by thickness.

Should I multiple 1.125(considering manufacuring tolerance) by control thickness to convert to nominal thickness?

 
Replies continue below

Recommended for you

See thread378-427039
Please review the definition in the standard you are building to.
You will be better served adding a sketch to your table, as there is not a consistent relationship between the two thicknesses.
 
It's not a good idea to PWHT with an Excel table. The best practice is to use the tables for each code. Don't forget Preheat.

Regards
 
Considering that some pipe specs use -12.5% with the '+' side only limited by the next heavier schedule,
while others are minimum wall specs with a -0 and '+' being the next heavier schedule.
You really need to look at each case.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
Be careful. See UW-40(f)definition of thickness.

Regards
 