We have some issues when the slurry pipes are left full of this material and these pipes are not in use, then the material starts to settle and gets hard which makes unavailable these slurry pipes for using them again. We have had stops and delays in the kiln for this matter and these issues get worse when having low ambient temperatures and the slurry pipes freezes out.
The objective of the project is to come to a practical solution in order to ensure the reliability of these slurry systems, taking into account the maintenance, environmental and process impact for what ever the solution is going to be.
Thank you for the help!!