hi,

how can i check elongation/strain on SMA wire during tensile?


Thanks
 
Like you would any wire?
Most wire people put ink marks on the wire or small tape flags and then measure elongation with optical trackers.
I have done this with wire that only had 0.5% elongation at fracture.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
Thanks Ed for the reply,

if using optical trackers, can it track the mark on the wire if the wire move to other position? in my case, the wire is subjected to shear loading (eg: as attached).


 
 https://files.engineering.com/getfile.aspx?folder=6debed8d-b4ea-4380-923f-d44e95b3017a&file=2018-12-06_11h25_04.png
Not the old units, but I presume that the technology has improved significantly.
You might need to talk to optical guys that are not in the testing business, but I am sure that it can be done.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
Strain gauges use the change in electrical resistance of wire to measure strain. You have a wire, so ...
 
Contact your local testing lab.