Jun 20, 2006 #1 Woody7 Industrial Joined Jun 20, 2006 Messages 1 Location US We have a building project in which we want to bond a 1" thick cast glass piece to a granite pillar in a outdoor plaza area. Recommendations?
We have a building project in which we want to bond a 1" thick cast glass piece to a granite pillar in a outdoor plaza area. Recommendations?
Jun 21, 2006 #2 nbucska Electrical Joined Jun 1, 2000 Messages 2,191 Location US If the thermal expansion is the same, it may be possible but even then within i" you can develop significant thermal stress, since the granit may act as heat sink. Plesae read FAQ240-1032 My WEB: <http://geocities.com/nbucska/> Upvote 0 Downvote
If the thermal expansion is the same, it may be possible but even then within i" you can develop significant thermal stress, since the granit may act as heat sink. Plesae read FAQ240-1032 My WEB: <http://geocities.com/nbucska/>
Jun 23, 2006 #3 ourious78 Marine/Ocean Joined Jun 23, 2006 Messages 10 Location US Is the Granite polished or rough?? Upvote 0 Downvote