I was wondering how much certain metals or more specifically aluminum expand when they oxidize.
On site we encountered a large pit on a submerged aluminum pipe. The pit was about 7.06 cm^3 in volume (if you were to approximated the volume as a hemisphere), after removing the corrosion the only thing remaining was a dimple of about 0.26 cm^3. This would give the corrosion an expansion ratio of over 27 which seems a bit high to me.
Cheers,
Alex
I was wondering how much certain metals or more specifically aluminum expand when they oxidize.
On site we encountered a large pit on a submerged aluminum pipe. The pit was about 7.06 cm^3 in volume (if you were to approximated the volume as a hemisphere), after removing the corrosion the only thing remaining was a dimple of about 0.26 cm^3. This would give the corrosion an expansion ratio of over 27 which seems a bit high to me.