Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

How good is an E-KOTE protection on a condenser coil. in an industrial and coastal area.

Status
Not open for further replies.

hollandhvac

Mechanical
Joined
Feb 23, 2007
Messages
120
Location
NG
Hello,

We are having a problem here with our condenser coils on our chiller system. The standard copper / al coil with blygold treatment is corroding and need to be replaced with coil with a better protection.
We have suggested to replace it with a coil with a Carrier E-coating, but our contractor is suggesting an E-KOTE, this is a shine coating with a green colour. The problem is I have never seen this coating and cannot find any details of it on the net.
My question is, if you know this coil protection, how well does it behave in an industrial and coastal area.
 
I just typed E-KOTE on my computer and a whole bunch of sites showed up. Once you identify the manufacturer, discuss the situation with them.
 