AUSTER
Mechanical
- Mar 9, 2010
- 5
I have been asked to install a 50NB stainless steel pipeline to carry air at 7 bar. This is categorised as "Sound Engineering Practice" (here in South Africa) but what does this specifically mean?
My client wants me to weld without purging to reduce costs. The pipe would not leak but I would not be complying with B31.3 as far as welding standards are concerned. Any relevant comments would be appreciated.
My client wants me to weld without purging to reduce costs. The pipe would not leak but I would not be complying with B31.3 as far as welding standards are concerned. Any relevant comments would be appreciated.