I am try to understand How do the polish parameter(use Polish machine,Polish Jig,polish Pad) affect the optical connector's (SC,LC)geometry (Curve of Radius,Apex offset,fiber protrusion).
I have done some test and got some result,but do not sure they are right or not.
1.Hardness of Polish Pad:
high hardness will get large Curve of Radius ?
2.High polish pressure:
high pressure will get large fiber protrusion but poor(large) Apex offset?
3.Polish time :
Longer polish time will get large fiber protrusion and good(samll) Apex offset?
4.More new jig and new pad can get good(samll)Apex offset?
(I guess may be more older jig port will have micro shaking when polishing because of wear).
I am try to understand How do the polish parameter(use Polish machine,Polish Jig,polish Pad) affect the optical connector's (SC,LC)geometry (Curve of Radius,Apex offset,fiber protrusion).
I have done some test and got some result,but do not sure they are right or not.
1.Hardness of Polish Pad:
high hardness will get large Curve of Radius ?
2.High polish pressure:
high pressure will get large fiber protrusion but poor(large) Apex offset?
3.Polish time :
Longer polish time will get large fiber protrusion and good(samll) Apex offset?
4.More new jig and new pad can get good(samll)Apex offset?
(I guess may be more older jig port will have micro shaking when polishing because of wear).