YesSimple stamping / forming process from a piece of flat steel.
Looks like a plate with a large hole in the middle of it?
I only need to make 4 pieces. I thing forming will be expensive.Simple stamping / forming process from a piece of flat steel.
Looks like a plate with a large hole in the middle of it?
Spend enough money and yes it can be.
Thank you GregLocock. If make it from segments and then weld, then maybe it will make it easier to manufacture?Metal spinning and laser trim seems pretty doable. You could hydroform it, but would have to find a vendor with a 50" hydroform. Probably could get away with pretty cheap tooling for the hydroform, then laser trim, once again.
Thank you JStephen. I can expand tolerances. If make it from segments and then weld, then maybe it will make it easier to manufacture?If those tolerances are critical, your best bet might be to start with a >44 mm disk and just machine the whole thing out of it.
Otherwise, take a good look and see if you can alter shape and/or tolerances.
For example, you can readily buy dished heads, where the whole thing is formed to a radius. You can buy flanged-only heads, where the center is flat and the edge is formed to a tight knuckle. You can get cones fabricated fairly readily. But none of those is going to meet a 0.3mm tolerance, either.
If you're going to specify the depth to a tight tolerance, you should probably show more exactly what the outer edge looks like, whether a sharp corner or what.
Thank you dvd. If make it from segments and then weld, then maybe it will make it easier to manufacture?Metal spinning and laser trim seems pretty doable. You could hydroform it, but would have to find a vendor with a 50" hydroform. Probably could get away with pretty cheap tooling for the hydroform, then laser trim, once again.