Hi all
We are building a new house and I work away for long periods. This trip home I noticed a crack in the kitchen area that to me looks quite alarming.
Crack is about 1mm wide and runs for approx 4 meters from the fridge recess to the external doorway.
Cannot tell if the crack is stable or still growing.
We plan to install large 900 x 600 tiles through this area and I am worried that they will crack down the track if the concrete continues to move.
Has anyone had any experiences with house cracks before.
Should I be concerned
Builder says that these are settling cracks. Easy answer from them.
First post so I hope the photos attached OK
Thanks
Ian H
We are building a new house and I work away for long periods. This trip home I noticed a crack in the kitchen area that to me looks quite alarming.
Crack is about 1mm wide and runs for approx 4 meters from the fridge recess to the external doorway.
Cannot tell if the crack is stable or still growing.
We plan to install large 900 x 600 tiles through this area and I am worried that they will crack down the track if the concrete continues to move.
Has anyone had any experiences with house cracks before.
Should I be concerned
Builder says that these are settling cracks. Easy answer from them.
First post so I hope the photos attached OK
Thanks
Ian H