Hello all

we are constructing a 48" crude oil line in accordance with ASME B313. we'll take a branch from existing line by a hot tap operation.

How can I find an information about at what temperatures does the impact have to be carried.

thank you all.

 
Replies continue below

Recommended for you

By ascertaining the minimum design temperature of the piping (if it is a pipeline you would be using B31.4) and consulting B31.3.

Steve Jones
Materials & Corrosion Engineer
 