Jan 20, 2010 #1 OSUengr Materials Joined Dec 21, 2009 Messages 8 Location US Could 1" thick Nickel 200 in the hot rolled/ hot rolled condition cause problems with welding, such as an increased possibility of weld solidification cracking or HAZ liquation cracking? Thank you.
Could 1" thick Nickel 200 in the hot rolled/ hot rolled condition cause problems with welding, such as an increased possibility of weld solidification cracking or HAZ liquation cracking? Thank you.
Jan 20, 2010 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US No, not from the joining literature I have reviewed for Nickel 200. Go here for some background information http://www.specialmetals.com/products/nickel200.php Upvote 0 Downvote
No, not from the joining literature I have reviewed for Nickel 200. Go here for some background information http://www.specialmetals.com/products/nickel200.php
Jan 21, 2010 Thread starter #3 OSUengr Materials Joined Dec 21, 2009 Messages 8 Location US Thank you. Upvote 0 Downvote