Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Hot Dipped Galvanized vs Painted structural steel in cold environments

Status
Not open for further replies.

Material98

Materials
Jan 24, 2018
2
Please advise. Can we use Zinc based paint system instead of Hot Dip Galvanizing for Structure Steel items in cold environment?
 
Replies continue below

Recommended for you

Yes, but hot dipped galvanizing is better than almost all other coating systems.
 
Depending on what kind of cold environment, the alternative of no coating system may also be acceptable. We are currently building a piece of equipment for northern Alberta which has no coating system on structural steel at the request of the client- because in practice, no coating system is required for medium term durability in that environment.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor