Hot dipped galvanised bolts? really?.... 9

Status
Not open for further replies.

Thedraffy

Structural
Joined
Sep 4, 2012
Messages
4
Location
GB
One of the design engineers (the lead) in the office has made a change to a set of drawing notes to the tune of: BOLTS AND WASHERS TO BE ZINC NICKEL ELECTROPLATED and replaced this with HOT DIPPED GALVANISED...

Am I correct in saying that bolts are not actually hot dipped galvanised... as they would be covered in a thick layer of zinc and the nut would not fasten?

that’s why bolts that require a "galvanised" finish are electroplated.... i.e. a thin layer of zinc is bonded to the bolt surface.

Cheers,

The Draffy

TheDraffy
 
No. You are not correct. Consult BS 7371-6 and ASTM F2329 amongst others.

Steve Jones
Materials & Corrosion Engineer


All answers are personal opinions only and are in no way connected with any employer.
 
Thanks Steve,

Appreciated

C


TheDraffy
 
To add to Steve's comments, structural applications frequently use thick hot dip galvanized coatings. The nuts are overtapped to accommodate for the increased coating thickness. Standards such as ISO 965-5 have been created to address this (tolerance class 6AZ).


 
Some of the structural guys have started pushing for mechanically galvanized bolts instead of hot-dip for more reliable tensioning. I prefer hot-dipped for the improved corrosion protection versus mechanically galvanized. Mechanical galvanizing is a porous coating, while hot-dip is effectively solid.

Zinc plating is typically very thin and provides minimal corrosion protection.
 