Hi my friends,

I would like to know if there is a standard or mandatory requirement for using hot-dip galvanization for stud bolts in piping. When can cold galvanization be used instead? Is this coating allowable in process piping within refineries and petrochemical facilities?

I prefer to use hot-dip galvanization for my project, but our documentation does not specify whether to use hot-dip or cold galvanization. I am searching for relevant references.

Thanks a lot!
 
AFAIK, corrosion protection for bolts and nuts is a choice, not a requirement of a code. You will often see it in company specifications and requirements but not in a design code.

Galvanising stud bolts is a bit hit and miss as the coating often becomes damaged and is then "touched up" with cold Galvanising material
 
Hot Dip Galvanising was (almost) a standard requirement for valves used in the north sea offshore oil and gas industry. There are various standards how to apply it. The major one being ISO 10684.
 
Spin dip ASTM F2329 tends to give better results. As you mention “Petrochemical” watch out for flange temperatures.
 
Cautions on hot-dip galvanizing high-strength structural bolts and temperature limits on galvanized bolts - you can extrapolate to your situation.

AISC galvanizing structural bolts.JPG

ASTM A-194 maximum service temperature for plated fasteners.JPG
 
Zinc-aluminum flake coatings outperform hot dip galvanizing and can be used on all strength classifications.
 
Zinc-aluminum flake coatings outperform hot dip galvanizing and can be used on all strength classification
Thank you for your response. I am looking for the applicable standard or regulation that mandates the use of hot-dip galvanized coating versus cold coating in gas and oil field applications Do you know any standards related to this?
 
Having worked in oil and gas industry in past, AFAIK , galvanized bolt is not a mandatory requirement but if the chosen coating is zinc coating , it shall be hot dip galvanized.
I looked PIP PNSM0120.

the relevant statement ' .. galvanized bolting shall be hot dipped in accordance with ASTM A153.
 
Thank you for your response. I am looking for the applicable standard or regulation that mandates the use of hot-dip galvanized coating versus cold coating in gas and oil field applications Do you know any standards related to this?
You'll be looking for a long time because it doesn't exist.

COMPANY standards may exist which require this, (Shell, ExxonMobil, BP, Total etc), but no such standards or regulation exists.

Why do you think such a thing exists or is this something you've been told without that person giving you the reference?
 
You'll be looking for a long time because it doesn't exist.

COMPANY standards may exist which require this, (Shell, ExxonMobil, BP, Total etc), but no such standards or regulation exists.

Why do you think such a thing exists or is this something you've been told without that person giving you the reference?
Thanks for your attention.

My friend works in a company, and in our specifications, it does not specify whether to use hot-dip or cold galvanized stud bolts. He thinks hot-dip galvanization is better. However, since the cost of cold galvanized is cheaper, he wants to refer to a standard that requires his company to use hot-dip galvanization
Can you help me
 
"and in our specifications, it does not specify whether to use hot-dip or cold galvanized stud bolts"

So change your specification.

A193 grade b7 is the material of the bolt. Doesn't address the coating which is specified in YOUR specification.
 
Or out of left field, you can use PTFE or XYLAN coatings. We commonly use these in chemical plants for the harsh environments.
 