jgeer
Automotive
- May 12, 2010
- 1
I am trying to brand a logo into natural rubber flooring. I am using a 400 Watt electric branding iron. I am able to successfully brand the rubber. Prior to branding the rubber does not rub off onto the hands or any other contacted surface. After the logo is branded into the rubber, the rubber rubs off after cooling down. The rubber is made from 100% recycled tires. I contacted the manufacturer, they had no suggestions.
I need to stop the post-branded rubber to solidify and stop rubbing off.
I have tried cleaning the branded area with regular household cleaners with no success. I have not tried acetone or the like since acetone melts rubber.
Any thoughts?
I need to stop the post-branded rubber to solidify and stop rubbing off.
I have tried cleaning the branded area with regular household cleaners with no success. I have not tried acetone or the like since acetone melts rubber.
Any thoughts?