I did a parking garage inspection a few weeks ago where in the driving surface in supported with Hollow-core Panels/planks. The garage is 3 storys and incurred a good bit of damage from Hurricane Harvey flood waters.
Nonethless, there were several Hollow-core panels with large longitudinal full length cracks along the bottom of the members. The cracks were faulted and there were already some signs of deflection. I've had some experience with collapsed Hollow-core panels in the past so I recommended shoring the panels to prevent complete failure.
Anyway, the client would like out-right replace the panels and this is where my lack of experience is hurting me. The dimension of the panel are 3'6" wide by 34'-6'' span length (inside to inside) (could be 35 or 36 end to end). Depth the panel I couldn't confirm, but based on the dimensions I took looks to be either 6'' or 8'', with a 2'' or 4'' topping slab.
So here's my silly question: where can I locate the load tables for a 3'-6'' wide panel? Everywhere I look the tables are 4' or 8'. I'm assuming since the load tables are given in PSF, then the width of the panel is far less critical than the length and depth, but I want to make sure before I specify something incorrectly. Is is something I should talk to a manufacturer about?
Nonethless, there were several Hollow-core panels with large longitudinal full length cracks along the bottom of the members. The cracks were faulted and there were already some signs of deflection. I've had some experience with collapsed Hollow-core panels in the past so I recommended shoring the panels to prevent complete failure.
Anyway, the client would like out-right replace the panels and this is where my lack of experience is hurting me. The dimension of the panel are 3'6" wide by 34'-6'' span length (inside to inside) (could be 35 or 36 end to end). Depth the panel I couldn't confirm, but based on the dimensions I took looks to be either 6'' or 8'', with a 2'' or 4'' topping slab.
So here's my silly question: where can I locate the load tables for a 3'-6'' wide panel? Everywhere I look the tables are 4' or 8'. I'm assuming since the load tables are given in PSF, then the width of the panel is far less critical than the length and depth, but I want to make sure before I specify something incorrectly. Is is something I should talk to a manufacturer about?