Any suggestions to drill about a 3/4" hole through a rubber stopper? I'm thinking a really fine tooth one, but I haven't done this before. About a 2" deep hole.
 
Get the kind used for cutting ceramics/concrete, with the abrasive where the teeth normally are. Oh, and try putting the rubber in a deep freeze before cutting.
 
Ironically enough, that's just what I put on order yesterday! Glad I'm going the right route. I'll confirm if this works for me
 
All of the hole cutters for rubber that I have used or seen are thin walled tubes with a sharp bevel on the end. The tube is slowly rotated as it is pressed into the rubber. A little oil will greatly reduce friction during cutting. I actually had to make one a few weeks ago. It was easier to make one than to order one.

 
We had some production guys try to open a .375 hole to .500 in a chunk of rubber. They ran a .500 bit into the hole and it remained .375. They froze it and then tried the drill again. Same result. I don't know if they tried liquid nitrogen. They did try heating a .500 rod red hot. Don't try that. It took a while to air out the 250,000 square foot high-bay factory area.

I would definitely go for the thin walled tube with an external bevel. Use care in retaining the part so the hole is the correct shape after release.
 
Using a diamond tipped core bit worked beautiful! Water and soap as lubricant.
 
Did this in College to make rubber feet for some equipment. Freeze the rubber with dry ice, then drill.
 
FWIW, CPros is (as usual) not wrong, but the abrasive tipped tools just work faster than sharp clean edges, and with less compression/distortion of the rubber occuring, so they tend to cut (abrade) a straighter hole, if messier due to rubber crumbs getting everywhere. Also, rubber is annoyingly good at making sharp steel tools dull very quickly...
 
I also did not have to freeze. Just a diamond coated hole saw. Same bits I use for glass. Came out pretty straight using a cordless drill, I need to get a drill press.
 
Many years ago I worked for a company that machined rubber, holes were cut with an abrasive saw under a flood of coolant, the coolant carried away the rubber crumbs,
B.E.