Hi...All ..!! Warm good morning to you..
Currently we are facing sever problem on following :
1.Heavy Naptha Unionfining reactor (HNUU) Pressure drop is increasing since last couple of months from 1.8 to 3.6 kg/cm2g (existing),still increasing trend.
We process naptha from Crude units/VGOHT /DHT units as well as imported naptha from Tank farm :
Total processing throughput of reactor : 660 m3/hr with FBP of 165- 168 C.We are now analyzing root cause of the problem.
Feed to the HNUU reactor which is single bed reactor with around 120 MT CO/MO Catalyst bed.Feed to the reactor is from Naptha spiltter bottom and out of 660 m3/hr majority around 240 m3/hr is from CDU unit itself.
Generally, we don't carry out regular daily testing of contaminatns in the Naptha from CDU/VGOHT/DHTs like Fe,Chloride etc.but we have carried out test of Particulate matters in all naptha of all units during last 3 days in naptha including Imported naptha too mostly they fall in the range of avg. 10 - 30 ppm.Imported naptha (avg.8.7 ppm).
We have also analysed the Boot water PH,Fe analysis of CDU o/h reciver ,VGOHT fractionator,stripper o/h,DHT stripper o/h & from those datas also it is very difficult to get the clue about that what is that causing fouling in the HNUU reactor/from where particulate matters /Fe etc. takes place.
Increasing Detla P in HNUU Rx otherwise will lead Unit shutdown.
I request you to give your opinions on this.
Regret for long description.
Thanks to all of you...!!!
Currently we are facing sever problem on following :
1.Heavy Naptha Unionfining reactor (HNUU) Pressure drop is increasing since last couple of months from 1.8 to 3.6 kg/cm2g (existing),still increasing trend.
We process naptha from Crude units/VGOHT /DHT units as well as imported naptha from Tank farm :
Total processing throughput of reactor : 660 m3/hr with FBP of 165- 168 C.We are now analyzing root cause of the problem.
Feed to the HNUU reactor which is single bed reactor with around 120 MT CO/MO Catalyst bed.Feed to the reactor is from Naptha spiltter bottom and out of 660 m3/hr majority around 240 m3/hr is from CDU unit itself.
Generally, we don't carry out regular daily testing of contaminatns in the Naptha from CDU/VGOHT/DHTs like Fe,Chloride etc.but we have carried out test of Particulate matters in all naptha of all units during last 3 days in naptha including Imported naptha too mostly they fall in the range of avg. 10 - 30 ppm.Imported naptha (avg.8.7 ppm).
We have also analysed the Boot water PH,Fe analysis of CDU o/h reciver ,VGOHT fractionator,stripper o/h,DHT stripper o/h & from those datas also it is very difficult to get the clue about that what is that causing fouling in the HNUU reactor/from where particulate matters /Fe etc. takes place.
Increasing Detla P in HNUU Rx otherwise will lead Unit shutdown.
I request you to give your opinions on this.
Regret for long description.
Thanks to all of you...!!!