how long to wait after pwht to do a RT on A106 wet sour service.

Status
Not open for further replies.
Joined
May 24, 2024
Messages
2
Location
CA
Hello i am working in fort mcmurray canada, i can not find anywhere in b31.3 where the RT of a PWHT wet sour service has a requirement of waiting 24 hrs after pwht for a rt to take place. So is there that requirement in any other code? the client is pushing hard to perform the rt right after the welding is done.
 
Can’t think of a code that would stipulate such a commercially contentious requirement off hand. It is usually contained in end user specifications.

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 