Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Historical Joist Data 30H9

Status
Not open for further replies.

ChrisKn

Structural
Mar 26, 2005
19
I've searched everywhere in our office for joist data on these specific sizes and it looks like we need to order the 75 year manual from the SJI. Right now we only have the 5o year manual which only has joists in the H series going up to 24H8. Anyway i was wondering if anyone would be able to pass along the information (resisting moment in inch-pounds) and (maximum end reaction in pounds) for this one particular joist (30H9), until we are able to order the newest manual?

Thank you ahead of time for your help.

Chris
 
Replies continue below

Recommended for you

Effective from 1974 to 1986:

30H9:
Resisting Moment = 1,075,000 in-lbs
Max. End Reaction = 7500 lbs
Approximate Wt = 15.4 lbs/ft
 