I am looking for any information on hilite installation in clearance fit holes. The stackup is aluminum/aluminum/CRES Specifically if anyone has experienced movement or "working" on this type fastener in a highly loaded or pressurized joint. The condition is noted by swirl marks in the paint on the fastener heads. Flush head fasteners. Thanks for any input.
 
don't install fasteners into out of spec holes. there's no such thing (IMHO) as installing a HiLite into a clearance hole, as the spec requires a small interference. If the hole is too large then use an oversize HiLite.

another day in paradise, or is paradise one day closer ?
 
MrBdude...

Hi-Lok [HL] pins/collars were originally designed for installation same as swaged-collar lock bolts and nuts/bolts: clearance fit in good-quality drilled tolerance holes. For this reason don't spend Your fastener budget for Hi-Lite pins when HL pins are 'good-enough'/better-than Hi-Lites in the application You describe.

HL pins do NOT tolerate installation in true interference-fit applications: The shank-to-thread transitions are rather sharp-edged so don't install HL pins in anything more than 'net-fit' [Boeing: transition fit] applications. In true interference fits, HL pin shoulders tend to damage undersized holes when shoved down the holes. NOTE: every bolt design has this same quirk... sharp transition shoulder between shank and threads. Then only practical way to install HL pins and flush/protruding head bolts of all kinds [with precision Dia shanks] into interference fit is by using 'shrink-fit'/freeze-fit methods [preferably dangerous liquid nitrogen]... and even this method requires the mechanics to become 'paper-hanging acrobats'.

The next evolution pin/collars were Hi-Tigue [HT]... which are like Hi-Loks in every respect... EXCEPT the shank-to-thread transition shoulder has a rounded bulge... and are intended for installation in true interference fit application. 'In-Theory' the rounded bulge facilitates installation in high interference fits... by 'stretching/smoothing/rounding' the hole surface [improving the hole quality and lightly cold-working the hole (?)] when the pin is pushed/pressed into position. HT Collars are also designed to facilitate tight-seating of the fasteners [heads] in-position even with the forces of interference in-play.

Hi-Lite [HLT] pins, on the other-hand are an evolution/merging of HL Pin and HT pin designs... and redesigned aspects for the collars. HLT pins are essentially HL pins with a rounded [not bulged-rounded] shank-to-thread transition edge... so it smoothly and 'non-abusively' installs in interference fits. Further, HLT pin/collar internal/external threads and internal depressions/cut-outs are designed to reduce mass in –combinations with higher strength alloys. HLT pins/collars are match-re-sized in various aspects to allow for significant mass reductions in the installed combinations...with very good installed strength and durability.

NOTE: these are the 'Reader's Digest' version' of HL, HT and HLT pin/collar evolution/technology.


Regards, Wil Taylor

o Trust - But Verify!
o We believe to be true what we prefer to be true. [Unknown]
o For those who believe, no proof is required; for those who cannot believe, no proof is possible. [variation,Stuart Chase]
o Unfortunately, in science what You 'believe' is irrelevant. ["Orion", Homebuiltairplanes.com forum]
 