I'm working on a high voltage insulating, high temperature ~300c prototype device.

PEEK is currently being used as an insulator in the device, does a higher temp resilient insulating material exist besides ceramic?

Thanks all!

Cameron
 
Replies continue below

Recommended for you

Above about 300C all carbon bonds become unstable so it's hard to go above that number. Try looking up Torlon.

Chris DeArmitt PhD FRSC
President

Plastic materials consultant to the Fortune 100
 
Thermosets - Urea formaldehyde or phenolic types.

(Torlon requires considerable post-moulding thermal cycle cross-linking)

H

www.tynevalleyplastics.co.uk

Politicians like to panic, they need activity. It is their substitute for achievement.
 
Take the 1st thing Chris said, no carbon bonds are going to survive long at that temperature (even ptfe will break down). You are in ceramic land.
 
Cool, thanks for the input guys- I am stoked to have your brain time.
 