We are currently investigating a replacement bushing material for C95400 aluma bronze. Our application operating temperatures are now reaching 1300° which is far above the maximum operating temperature of the C95400.

For the application, the bushing is pressed into a cast iron housing. A 303 stainless shaft travels through the bushing, there is very little load on the shaft and the shaft only rotates 90° back an forth about 5 times a minute.

We were considering using Nitronic 60 for its high temperature service properties as well as its anti galling properties.

Any other ideas are appreciated.




 
We didn't have much success with Nitronic 60 above 1000F. Not saying it want work at your temperature but under our conditions it didn't

I would try to use a CI bushing from ASB with a high temperature lubricant from ZYP. Do not use graphite or moly as your temperature is too high.



What is your operating environment?

Is the 1300F the max or is it a continuous temperature?
 
Sorry the 1300° is the maximum temperature would see. Standard operating temperatres would be in the range of 600°-700°.

The assembly sits in the exhaust of a diesel engine. So you would have plenty of carbon soot, moisture, CO... expelled from the engine.



 