Appreciate the link to the report.
Talking point;
One thing that about the failure is the amount of distortion of
the shell. All the failures from HTHA I've seen had very little
distortion at the failure size, The only failure that unzipped
the vessel along the welds and HAZ was one that was caused
by an internal explosion. HTHA was confirmed a long the
fracture surface.
blacksmith37,
I'm sure that Shell took HTHA as a possibility based on the
1950/1954 "Shell Corrosion Data Survey" by Nelson, "The Red
Book" which had some curves on the potential for H2 damage
in several steels. My boss at the time almost paranoid about
H2. He was always on the phone with someone at Shell
Development. I assume this was Nelson at Shell. Our site had
two H2 plants and 3 processes that used H2 with 2 of them
skirting the potential fro H2 damage.