I need sources of high temperature ceramic boards, fibers and blanket and their support system. We are talking for about 1700 deg. C. materials. Can anybody help?

Regards,

LCE
 
Replies continue below

Recommended for you

If you need high purity alumina insulation material (because your process is in hydrogen atmosphere) than contact Zircar Ceramics They have a variety of HA boards, from ZAL-15AA (15pcf), AL30-AA (30pcf) to ZAL-45 (45pcf).
Unifrax at has also a variety of alumino-silicate boards, blankets and bulk fibers that will suit your needs.
 
Thanks you all, for your info. I bought Zircar AL25 for hotface. May use Unifrax for subsequent layers.

Warmest regards,

LCE
 