Guys,
I am designing a Section VIII-1 heat exchanger with design conditions 1058°F at 80 psig. I am using SS321H. While I do have all the stress values for SS321H at this temperature from Section II-D, Section II-D does not provide yield stresses for any materials over 1000F, which is causing Compress to crash. Does anyone have any suggestions for handling this?
I am designing a Section VIII-1 heat exchanger with design conditions 1058°F at 80 psig. I am using SS321H. While I do have all the stress values for SS321H at this temperature from Section II-D, Section II-D does not provide yield stresses for any materials over 1000F, which is causing Compress to crash. Does anyone have any suggestions for handling this?