I am working on a project & using following high temperature alloys to build furnace rolls and it looks like it is out of budget, does anybody know the material cost of these alloys? If so, please share. Thank you.
(1) HN (G-X35NiCrSi25-21 OR Pyrotherm G24/24 NbTz)
(2) HP Modified (G-X40NiCrSiNb35-26 OR Pyrotherm G25/35Nb)
(1) HN (G-X35NiCrSi25-21 OR Pyrotherm G24/24 NbTz)