High Temp Elastic Modulus 3

Status
Not open for further replies.

Metalmeister

Nuclear
Joined
Mar 4, 2008
Messages
62
Location
US
Would someone know of a source/link to data on the elastic modulus and Poisson's ratio for AISI 304 and Ductile Iron at 1400°F. Thanks.
 
Metalmeister;
Regarding the elastic modulus for 3XX austenitic stainless steel, one source is ASME B&PV Code, Section II, Table TM-1.
You can interpolate the value yourself based on

1400 deg F 19.2 psi x 106
1500 deg F 18.1
 
Other than the Code the only source that I use in an ASM publication: High Temperature Property Data: Ferrous Alloys, ed. M. F. Rothman, ISBN: 0-87170-243-6

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
Thank you Metengr and Edstainless for your helpful responses.
 