High Strength Anchor Rods

Status
Not open for further replies.

dik

Structural
Apr 13, 2001
26,057
Looking for a source/specification for high strength stainless steel anchor rod material (1" dia or larger) to be used with a heavy hex nut threaded on the embedded end. Corrosion resistance similar to 316L.

Any suggestions for a spec'd material and/or source.

Dik
 
Replies continue below

Recommended for you

What material did you use in coming up with the 1" dia. call out?.
What is the standard you are working to?

Come back with a few more details of your requirements as to strenght, corrosion resistance, etc.

Depending on your strength requirements you could use 316 class 2 (strain hardened) material. I have recently seen 2205 used for anchor rods.

I would contact Portland bolt with your specific requirements.

 
from my notes:

STAINLESS STEEL

ANCHOR RODS SHALL CONFORM AISI 430 AND ASTM A276 HAVING A MIN FY = 50 KSI (350 MPA) AND A UTS = 75 KSI (520 MPA) OR APPD EQ

HIGH STRENGTH ANCHOR RODS SHALL CONFORM AISI 2205 AND ASTM A276 HAVING A MIN FY = 95 KSI (655 MPA) AND A UTS = 125 KSI (860 MPA) OR APPD EQ

ANCHOR ROD WASHERS SHALL CONFORM TO ASTM A240 AND NUTS SHALL CONFORM TO ASTM A594 U/N

ALL ANCHOR RODS SHALL BE [3/4"| 19]%%C GRADE 50 U/N. NUTS AND WASHERS TO MATCH

ANCHOR RODS DENOTED AS [1"| 25]%%C OR LARGER SHALL BE HIGH STRENGTH (GRADE 95). NUTS AND WASHERS TO MATCH

Dik
 
Look for 2205, it is a duplex stainless and will give you superior strength and corrosion resistance.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 