Feb 1, 2002 #1 Guest Where is a good source for high speed ceramic bearing (100,000 rpm). I found some sites but it seems like they only small sizes. Can you help me? Thank you.
Where is a good source for high speed ceramic bearing (100,000 rpm). I found some sites but it seems like they only small sizes. Can you help me? Thank you.
Feb 4, 2002 #2 butelja Mechanical Joined Jun 9, 1999 Messages 674 Location US Do you have any more specifics (size, load, etc.) for the application? Upvote 0 Downvote
Feb 4, 2002 #3 ecampos Mechanical Joined Dec 21, 1999 Messages 97 Location US Try KOYO bearings in Japan. They had a 115,000 rpm ceramic bearing when lightly loaded and using a oil lube not grease. Check them out. I am sure that they are on the WEB somewhere. Edson Campos edsoncampos@earthlink.net Upvote 0 Downvote
Try KOYO bearings in Japan. They had a 115,000 rpm ceramic bearing when lightly loaded and using a oil lube not grease. Check them out. I am sure that they are on the WEB somewhere. Edson Campos edsoncampos@earthlink.net
Feb 5, 2002 #4 butelja Mechanical Joined Jun 9, 1999 Messages 674 Location US FAG also has a large selection of hybrid ceramic bearings. Upvote 0 Downvote