Hello,
I have some carburized parts (AMS 6265 material) that exceed the hardness limit (gear area). Te requirement is max.63 HRC and the parts have around 64 HRC at .003 inch measured with HV0.5.My question is: Is it a small difference like 1-2 points HRC so detrimental to the parts? I am interested on studying this subject
Please share your opinions from your experience and knowlogies.
Thank you in advance!
I have some carburized parts (AMS 6265 material) that exceed the hardness limit (gear area). Te requirement is max.63 HRC and the parts have around 64 HRC at .003 inch measured with HV0.5.My question is: Is it a small difference like 1-2 points HRC so detrimental to the parts? I am interested on studying this subject
Please share your opinions from your experience and knowlogies.
Thank you in advance!