I am testing the upper limit of hall sensors and I would like a quick and simple way of generating a high flux field over 10,000 to 20,000 Gauss, over 1 Tesla in a gap about 4 mm (0.15") wide. The field needs to be reasonably even over about 10x10mm (0.4") so that I don't get too much variation with position.
At the moment I have two 1" Neo. magnets 0.5T at surface and separated by 4 mm. I am getting good field up to 1 T.
thanks
At the moment I have two 1" Neo. magnets 0.5T at surface and separated by 4 mm. I am getting good field up to 1 T.