I have a print with Worknorm 1.4122 on it the chemistry is as follows:
X35CrMo17 DIN
I am not able to find a common USA grade of SS that can fit this chemistry. The part is a sort of spring clip so it seems that I need a martensitic grade, however the Cr content in the above is much higher than in the martensitic grades like 420. I would like to avoid sugesting a PH stainless as there is no forming involved. Is there a high chrome grade similar to 420, or alternately is there an american grade I should recommend?
Thanks In advance.
nick
Code:
0.33-0.45 C:Carbon
=1.00 Mn:Manganese (nominal?)
=1.00 Si:Silicon (nominal?)
0.04 P:Phosphorus (max?)
0.015 S:Sulfur (max?)
15.5-17.5 Cr:Chrome
0.80-1.30 Mo:Molybdenum
=1.00 Ni:Nickel (nominal?)
X35CrMo17 DIN
I am not able to find a common USA grade of SS that can fit this chemistry. The part is a sort of spring clip so it seems that I need a martensitic grade, however the Cr content in the above is much higher than in the martensitic grades like 420. I would like to avoid sugesting a PH stainless as there is no forming involved. Is there a high chrome grade similar to 420, or alternately is there an american grade I should recommend?
Thanks In advance.
nick