Jun 10, 2002 #2 grayseal Materials Jun 29, 2001 78 abu, My guess would be Hydrogen Induced Cracking. Only a guess. grayseal Upvote 0 Downvote
Jul 18, 2002 #3 raghurambathula Materials Jul 18, 2002 4 hidrogen induced cracking this will be done as per NACE standrd TM-02-84 stressed specimen will be kept under corrissive atm. for a perticular period, normally 120 hours test conditions as per the above standard Upvote 0 Downvote
hidrogen induced cracking this will be done as per NACE standrd TM-02-84 stressed specimen will be kept under corrissive atm. for a perticular period, normally 120 hours test conditions as per the above standard