WHAT IS HIC testing criteria as per NACE
 
Replies continue below

Recommended for you

abu,

My guess would be Hydrogen Induced Cracking. Only a guess.

grayseal
 
hidrogen induced cracking this will be done as per NACE standrd TM-02-84
stressed specimen will be kept under corrissive atm. for a perticular period, normally 120 hours
test conditions as per the above standard
 