I have a ASTM F65 material, which is a low carbon steel.
It has been encountered a HIC crack during the testing, the crack is 40mm long and due to the orientation, it constitutes a failure.
The chemical has passed which is a quite clean material. What other reason can cause this HIC crack failure?
Thanks in advance!
I have a ASTM F65 material, which is a low carbon steel.
It has been encountered a HIC crack during the testing, the crack is 40mm long and due to the orientation, it constitutes a failure.
The chemical has passed which is a quite clean material. What other reason can cause this HIC crack failure?