We have an air cooler condenser in a Vacuum Hydrobon process unit. Operating temperature is 260ºC. Operating pressure is 55bar G. Hydrogen partial pressure is 670 PSI. Susceptible corrosion mechanisms are HIC, SSC, SCC, HCL and HTHA. The project specified for the air cooler tubes & headers, 1 ½ Cr ½ Mo steel with NACE requirements according MR 0175 & MR 0103 standards.
Because of difficulties in performing PWHT requirements for strength welds of 1 ½ Cr ½ Mo steel tubes into the tube sheets headers, we are suspicious about the materials project choice.
What proven steel materials in the above conditions would be an alternative to 1 ½ Cr ½ Mo steel?
An answer from the forum would be appreciated.
Best Regards
Luis Marques