I am working on one of its offshore project having field with wet sour H2S content . In data sheet of the slops tank ( UL-142 tanks D.P: 2.5 PSIG)& material showing HIC and SSC resistant. we are buying plate A516 GR 60 from Arcelor Mittal with HIC testing per NACE TM 0284 & Client specification and MTC states that material compliant to NACE MR 0175/ ISO 15156-2 & HIC test qualified
Also as per NACE MR 0175/ ISO 15156-2 section 7 Selection of pre qualified material resistant to SSC
" No additional laboratory testing of pre qualified material selected in this way require"

Now my question is

1) If the material is already Tested & passed for HIC test as per NACE TM 0284 & client specification also MTC stated for NACE MR 0175 / ISO 15156-2. DO we still required separate testing for SSC as per NACE TM-0177???.

As per my understanding for HIC qualification of plates it requires extra care during production phase of plate and SSC will automatically qualified once NACE MR 0175 section 7 calls for no separate testing as MTC already stated for HIC pass test result and compliance to NACE MR-0175/ ISO 15156-2. Also we have approached earlier a lot of mills but no one prepare to do both HIC & SSC testing on same plate with heat numbers saying only one test ( HIC OR SSC)can be performed. I have checked Client Specification which calls for HIC testing and Inspection for qualification but no separate specification for SSC specified. i dont want that at later stage client raise concern why plate is not SSC tested

Your valuable input will be much appreciate
 
Do not cross post with other forums. You have a response to your post.

thread794-423543
 
Sulfide stress cracking(SSC) is a special case of hydrogen stress cracking, also known as hydrogen-induced cracking(HIC). This cracking mechanism depends on several factors:hydrogen fugacity, material strength, heat treatment/microstructure, applied stress, and temperature. For many steels, there is a threshold stress exists below which HIC doesn't occur. This threshold stress is a function of material strength and the specific hydrogen-bearing environments. It is not a fixed value and hence can't to be referred to as "material property".

NACE TM0284 provide two solutions for HIC/SSC test: Solution A - NaCl+CH3COOH saturated with H2S, Solution B - a synthetic seawater solution with H2S. However, this standard doesn't include acceptance or rejection criteria. The test results are only for reference. According to our supply experiences, for ASTM A516 Gr.60/65/70 HIC resistant steels, CLR≤10%, CSR≤3%, CTR≤1% in Solution A; CLR≤10%, CSR≤3%, CTR≤1.5% in Solution B. “HIC Resistant” can be achieved by carefully control the chemical composition such as Ni<1%, C<0.20%, O<0.0025%, S<0.002%, P<0.009%, CE<0.42%.

This technical article may be more helpful: