Hetergenous Welding

Status
Not open for further replies.

redandysafc

Mechanical
Dec 18, 2005
60
Can anybody tell me what hetergenous welding means please
 
Replies continue below

Recommended for you

I believe it is another description for welding of dissimilar materials.
 
redandysafc,

I concur with metengr. If you will look into a materials dictionary, 'heterogeneous' means that the composition of a material can vary, as with composite materials; and as opposed to homogeneous. That is why you will see the term "heterogeneous welding" between duplex stainless steels or between dissimilar materials.
 