Hi all

For material A333-6 client rejected ER70S-6/E7018 And Ask using ER80S-Ni1 and E7018-1
Could you explain a little more
 
We are not the client. Ask the client.

"Everyone is entitled to their own opinions, but they are not entitled to their own facts."
 
They both meet -50 F impacts per their SFA/AWS A Specifications while the others do not.
 
Let me know where this pressure equipment will be installed, so I can be sure to give it a wide berth in my travels.