What the problem is that we have been told by our supplier
that there is porosity in the base metal and the zinc plating cannot stick to the part it usually take a couple of day for the so called white rust to appear
I have done a Materials engineering degree
but that has been a couple of years back
and i have never be involved in steel or iron manufacturing
when i was taking to the supplier he told that white rust come up after a couple of day after the iron has been plated
this is something that i find hard to believe
is there any exact way of measuring the Porosity
what is basically happening is that we submit plane iron and we get it platted with
Zinc and when we receive the parts there is a white staining on the zinc platting
do you know any way how Porosity can be measured ?
any info would be appreciated
that there is porosity in the base metal and the zinc plating cannot stick to the part it usually take a couple of day for the so called white rust to appear
I have done a Materials engineering degree
but that has been a couple of years back
and i have never be involved in steel or iron manufacturing
when i was taking to the supplier he told that white rust come up after a couple of day after the iron has been plated
this is something that i find hard to believe
is there any exact way of measuring the Porosity
what is basically happening is that we submit plane iron and we get it platted with
Zinc and when we receive the parts there is a white staining on the zinc platting
do you know any way how Porosity can be measured ?
any info would be appreciated