I need some help in regards to heat treating a camshaft of 52100.
- Currently we start with a round 2" billet, its roughly 6.5" long.
- Its rough machined, down to an effective diameter of about 1.25", with an eccentric lobe in the center (hence the 2" bar material). 0.020" is left on all ground surfaces.
- Part is heat treated to HRC60
This is where the problem occurs as the part moves all over the place. Hence the 0.020" left on all ground surfaces.
The heat treating company uses a oil quench.
Any ideas on how to prevent the movement.
- Currently we start with a round 2" billet, its roughly 6.5" long.
- Its rough machined, down to an effective diameter of about 1.25", with an eccentric lobe in the center (hence the 2" bar material). 0.020" is left on all ground surfaces.
- Part is heat treated to HRC60
This is where the problem occurs as the part moves all over the place. Hence the 0.020" left on all ground surfaces.
The heat treating company uses a oil quench.
Any ideas on how to prevent the movement.