I would appreciate any help identifying this material and a source where I can purchase it.
Chemical Composition (Nominal Analysis, Percent)
Carbon, max 0.10
Manganese 7.00 min. - 9.00 max.
Silicon 3.50 min. - 4.50 max.
Sulfur, max 0.030
Phosphorus, max 0.060
Chromium 16.00 min.-18.00 max
Nickel 8.00 min.-9.00 max.
Nitrogen 0.08 min.-0.18 max.
Mechanical and Physical Properties
Tensile Strength, ksi, min. 95
Yield Strength (0.2% offset), ksi. min. 50
Elongation in 2 in., (or4D), %,min. 35
Hardness, Brinell, max. 241
Rockwell B, max. 100
Density, grams per cu. cm. 7.62
Electrical Resistivity, microhm-cm 98.2
Modulus of Elasticity, tension, psi x 10-6 26.2
Thomas J. Walz
Carbide Processors, Inc.
Chemical Composition (Nominal Analysis, Percent)
Carbon, max 0.10
Manganese 7.00 min. - 9.00 max.
Silicon 3.50 min. - 4.50 max.
Sulfur, max 0.030
Phosphorus, max 0.060
Chromium 16.00 min.-18.00 max
Nickel 8.00 min.-9.00 max.
Nitrogen 0.08 min.-0.18 max.
Mechanical and Physical Properties
Tensile Strength, ksi, min. 95
Yield Strength (0.2% offset), ksi. min. 50
Elongation in 2 in., (or4D), %,min. 35
Hardness, Brinell, max. 241
Rockwell B, max. 100
Density, grams per cu. cm. 7.62
Electrical Resistivity, microhm-cm 98.2
Modulus of Elasticity, tension, psi x 10-6 26.2
Thomas J. Walz
Carbide Processors, Inc.