May 13, 2016 #1 sarmas Materials Joined May 5, 2016 Messages 5 Location GR WOULD LIKE IF SOMEONE THE CUTTING PARAMETERS FOR AMADA laser-2415 FANUC 1500W
May 16, 2016 #2 Km3l3on Industrial Joined Jan 11, 2016 Messages 8 Location RO Hi, I can share with you the cutting parameters from a LCG 3015 is you want Upvote 0 Downvote
May 16, 2016 Thread starter #3 sarmas Materials Joined May 5, 2016 Messages 5 Location GR IT'S THE SAME. I AM NEW TO WORK AND DO NOT KNOW MUCH .. WILL LIKE MUCH IF YOU CAN HELP Upvote 0 Downvote
May 17, 2016 #4 Km3l3on Industrial Joined Jan 11, 2016 Messages 8 Location RO The LCG 3015 is a 3500W Laser... I hope it helps you http://files.engineering.com/getfile.aspx?folder=e8b45d3e-5c54-4cc4-b333-9a1d24450a46&file=Processing_Conditions_LCG_AF3500IC_X41391A.pdf Upvote 0 Downvote
May 17, 2016 Thread starter #5 sarmas Materials Joined May 5, 2016 Messages 5 Location GR thanks i hope..... Upvote 0 Downvote
May 18, 2016 #6 jjl1210 Industrial Joined Jul 17, 2015 Messages 114 Location US Check out the post "Help with cutting parameters" it should help you. Upvote 0 Downvote
May 18, 2016 #7 Skinnedrabbit Industrial Joined Feb 15, 2016 Messages 8 Location GB Hi , Do you have any cut conditions for 4mm-5mm-6mm stainless on oxygen . I have the lc1212 1.5kw I've got up to 3mm stainless on clean cut somewhere near if you need them .thanks rob Upvote 0 Downvote
Hi , Do you have any cut conditions for 4mm-5mm-6mm stainless on oxygen . I have the lc1212 1.5kw I've got up to 3mm stainless on clean cut somewhere near if you need them .thanks rob