Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Helicoil Inserts for Plastics? 2

Status
Not open for further replies.

miner00

Mechanical
Sep 27, 2001
48
A vendor of mine is recommending that we use helicoil inserts for a threaded hole in a part made out of Delrin. Most of the information that I have suggests that brass inserts are better for plastic materials. Does anyone have experience with this or know of a good resource?

Thanks for any suggestions.
 
Replies continue below

Recommended for you

Threaded inserts, such as the brass-type that you mentioned, would be a better fit than the helicoil-type for threading into plastic. PSM is a good manufacturer of inserts; their website is
 
An even better supplier of inserts for plastics is Emhart Teknologies, located in Danbury, CT. They make both the Heli-Coil and the Dodge line of inserts for plastics which can be obtained in 360 brass, steel, aluminium and stainless steel. Worked with them on several applications, great company!

Dugu
 
Agreed! Emhart Teknologies is a good company. We use the Dodge products in plastic and have never had a problem. Their website is
 