We have and upcoming job where we will turn the flywheel, then we have to seat the gear ring on that flywheel. These will be short run parts. I have heard about taking an electric oven and rewiring it to run both the oven and broiler at the same time. Looking for help.
 
400 degrees will do it with a min of .005 to a max of .007 thousands interference a oven should work fine, or you can buy a Blue Max thermal oven on ebay for a few hundred bucks and it runs on 110v and heats to 500 degrees.

regards
 