Question for you guys.
On A572 gr. 50 and A514 steel.
Is it allowed to heat the steel and put wet rags on it to stop it from moving anymore. Or is it best to let it air cool and hope it doesn't move go past where you want it.
 
Replies continue below

Recommended for you

I appreciate the info. I'm just tired of telling these guys that they need to let it air cool not to put rags of water to cool it down. Epically on a514 steel for drilling rigs. If anyone know any real explanation on why it can't be done please feel free to pass on any further information.

Thanks
Qcpeewee
 
The last paragraph of the cited article talks about cooling.

TTFN
faq731-376
7ofakss

Need help writing a question or understanding a reply? forum1529

Of course I can. I can do anything. I can do absolutely anything. I'm an expert!
 