We have performed Cold Bending on SA213 T11 (P4) Material for Superheater tubes.
Dia of Tube is 31.8mm and Thickness in 3mm
Now what does the code say about Heat Treatment. Either we should perform heat treatment or not. If yes then please specify reference and what will be Temperature and Soaking Time.
We have performed Cold Bending on SA213 T11 (P4) Material for Superheater tubes.
Dia of Tube is 31.8mm and Thickness in 3mm
Now what does the code say about Heat Treatment. Either we should perform heat treatment or not. If yes then please specify reference and what will be Temperature and Soaking Time.