We have a 3/4" thk plate that we are rolling to 16" OD. material is SS 304. Per UHA 44 and strain is about 5%, and UHA 44 table is listing 304 material to be good up to 20% of strain.
Everything looks OK, however, my problem is design temperature of 250°C. UHA-44 table is referring to temperatures above 580°C. Am I missing something?
 
Replies continue below

Recommended for you

FSB01, what makes you think you are missing something?

Regards,

Mike
 
Well, it is UHA 44 Table. Design temperature range listed in the table is above 580°C. My design temp. is quite lower. Is there some other reference for cold forming of SS 304?
 
FSB01, you are not required to stress relieve. You are not prohibited from it either.

Regards,

Mike
 